                            21。 SOLDERING FLUID
For mending articles of tin; iron; zinc; copper; and almost all other 
metals。 Take 2 fl。 ounces of muriatic acid; add zinc till bubbles cease to 
rise; add 1/2 a teaspoonful of sal ammoniac and 2 ounces of water。 Damp 
the part you wish to solder with this fluid; lay on a small piece of lead; 
and with a piece of hot iron or soldering iron solder the part。

                            22。 SOLDER FOR TIN
Take of pewter 4 parts; tin 1 part; bismuth 1 part; melt them together。 
Resin is used with this solder。

23。 COLD METHOD OF SILVERING IRON WITH SILVER…PLATE
Polish the iron toy wish to silver; then damp it over with soldering fluid 
(receipt No。21) When this is done give it a coat of No。22 solder。 This is 
done by laying a piece of cold solder on the iron; and spreading it over 
with a heated soldering iron; when by this means you get the iron nicely 
plated with solder; then lay on your silver…plate evenly; and gently rub 
it over with the heated soldering iron; and it will become firmly united 
with the solder as the solder is with the iron; so that you have the iron 
beautifully plated with silver with very little cost or trouble。

24。 HOT METHOD OF SILVERING IRON WITH SILVER…PLATE
First polish the iron you wish to silver; wet it well over with No。21 
soldering fluid; then having procured that kind of silver…plate which is 
tin on one side and silver on the other; place it evenly on; with the 
tined side next to the iron; then place it on the fire until the 
silver…plate melts down; then at once take it from the fire; and it will 
be firmly attached to the iron; and will be excellent plate; yet No。23; 
the cold method; is to be preferred in most cases。

25。 SILVERING LOOKING…GLASSES WITH QUICKSILVER
Take a piece of marble or some other substance very smooth; true; and 
level; lay on this the glass you wish to silver; then make a ridge of 
putty on the marble against the edge of the glass all round it; so that 
you can pour quicksilver on the glass until it is all covered over; and 
will be prevented from running off by the ridge of putty; an inch or two; 
or three outside this ridge make another of putty; then cover the 
quicksilver on the glass all over with tin…foil; and press it firmly but 
cautiously against the glass until you have squeezed out all the 
quicksilver you can。 while you press this you may remove part of the first 
ridge of putty to give the quicksilver a chance of escape。 When it is well 
pressed against the glass there will be an amalgam formed of the tin…foil 
and the quicksilver that is left; which will firmly adhere to the glass。 
By this means you have a very beautiful and cheap looking…glass; the 
quicksilver that escapes; being saved by the second ridge of putty; may be 
used again。






26。 SILVERING LOOKING…GLASSES WITH PURE SILVER
Prepare a mixture of 3 grains of ammonia; 60 grains of nitrate of silver; 
90 minims of spirits of wine; 90 minims of water; when the nitrate of 
silver is dissolved; filter the liquid and add a small quantity of sugar 
(15 grains) dissolved in 1 1/2 oz。 of water; and 1 1/2 oz。 of spirits of 
wine。 Put the glass into this mixture; having one side covered with 
varnish; gum; or some substance to prevent the silver being attached to 
it。 Let it remain for a few days and you have a most elegant 
looking…glass; yet it is far more costly than the quicksilver。

                         27。 PATENT BURNING FLUID
To 1 gallon of 95 per cent。 alcohol; add 1 quart of camphene oil; mix and 
shake well; and if transparent it is fit for use; if not; add sufficient 
alcohol; shaking it well; to bring it to the natural colour of the 
alcohol。 It may be coloured to suit the fancy by adding a little tincture 
of golden seal; or any other colouring drug。 This receipt has been sold 
for 10。

                             28。 BURNING FLUID
Take 4 quarts alcohol; and 1 quart spirits of turpentine; mix well 
together; and it is ready for use。

29。 NON…EXPLOSIVE BURNING FLUID
Take 1 gallon 44 proof alcohol; 1 quart camphene; 3 oz。 of alum 
pulverized; 1/2 oz。 camphor gum; 65 drops cuicuma; mix all together and 
let it stand 12 hours; and it is ready for use。

                  30。 VINEGAR IN THREE DAYS WITHOUT DRUGS
Take 2 barrels and saw one of them in two in the centre; and put one…half 
on the top; and the other at the bottom of the whole barrel; (or you may 
use three whole barrels if you like。) The middle barrel is to be filled 
with maple; beech; of baswood shavings; which are to be planed from the 
edge of boards only two or three feet long; which allows the shavings to 
roll; and prevents them form packing tight; and also allows air to 
circulate through them; which is admitted through a number of inch holes; 
which are to be made near the bottom of the barrel and just above the 
faucet; which lets the vinegar run into the tub below。 The top tub has its 
bottom pierced with small bit holes; having several threads of twine 
hanging in them to conduct the vinegar evenly over the top of the shavings 
in the middle of the barrel。 Air must be permitted to pass out between the 
top tub and barrel; which comes in at the holes in the bottom。 The 
shavings which fill the barrel must be soaked three or four days in good 
vinegar before they are put in。 When thus arranged; for every gallon of 
water use 1/2 lb。 of sugar; (that you get from molasses barrels does vary 
well。) If you wish to make vinegar from whiskey; put in 4 gallons of water 
to 1 gallon of whiskey; and if from cider; put in one…third water; and 
fill the top tub with this fluid; putting 1 pint good yeast to each barrel 
making; and have the holes with threads or twine so arranged that it will 
run through every twelve hours; and dip or pump up with a wooden pump
every night or morning; and three days will make good substantial vinegar; 





which will keep and also improve by age。 Some use only 1 gallon of whiskey 
to 7 gallons of water。 This accounts for so much poor vinegar。 Make good 
vinegar; it will pay you。 If a few gallons of water if made boiling hot so 
as to warm the whole of a gentle warmth; it will make faster than if used 
cold。 This must be done in cool weather; and the room also should be kept 
warm。 For families; small kegs will do; but for manufacturers large casks 
are best。 Many make vinegar by just putting fluid into the barrels of 
shavings; soaked as directed above; and do not let it run through; but let 
it stand in the shavings till sour; but it does not work fast enough for 
manufacturers。 It will do where only a small amount is needed; keeping the 
same strength of fluid as for the other plan; which is best。 Two or three 
years ago; this receipt was sold for from 50 to 150。 If vinegar is made 
from whiskey; it will have a more beautiful color if 5 or 6 lbs。 of sugar 
is put into each barrel; of course keeping the same proportions of water 
as though only one kind was used。 The shavings will last the whole season。

                              31。 CUBA HONEY
Good brown sugar 11 lbs。; water 1 quart; old bee honey in t